A synthetic fiber filament which is composed of material containing 85 percent or more polyester thermoplastic resin. The resin which may be either thermoplastic or thermosetting. A polyester resin is created by the esterification condensation of dihydroxy alcohols and dicarboxylic acids. |
|
|
|
|
|
|
|
|
|
Today over 70 to 75% of polyester is produced by CP( continuous polymerisation) process using PTA(purified Terephthalic Acid) and MEG. The old process is called Batch process using DMT( Dimethy Terephthalate) and MEG( Mono Ethylene Glycol).
Speciality fibres available in Polyster:
- High /low shrink fibres
- Micro Denier
- Flame Retardant
- Cationic Dyeable
- Low Pill
- Anti Bacterial
- Super High Tenacity
- TBL-Trilobal
We offer 100% Polyester Yarn Spun on both Ring Spinning (R.S) as well as open end (O.E). All single yarns are auto coned/spliced & 2 told yarn are TFO Doubled-
- 100% Polyester Ring Spun Raw White- NE 6 to NE 80s- suitable for knitting & weaving.
- 100% Polyester multi-fold yarns in- NE 6 to 16-3 plies, 4 plies, 5 plies, 6 plies-available in R.S. as well as O.E.
- 100% Polyester sewing thread yarn-NE 20 to 50s on paper as well as perforated dye cones (Ring spun) using SHT fibre.
- 100% Polyester open end yarn-Ne 8 to 18
- 100% Polyester Yarn made from Mcro denier fibre 0.8D or 0.9D-Ne 20s to Ne 60s
- 100% Polyester Yarn optical white using optical white fibre- Ne 20s to Ne 36s
- 100% Polyester Ring Spun Yarns in dope dyed black color or any colour- Ne 12s to Ne 32s
Packing :
- Normal Knitting & weaving yarns on 1.8Kgs to 2.5Kgs cones.
- Multi fold yarns available also on Jumbo cones of 8" or 10" traverse of 4.5Kgs to 5.5Kgs cone weight.
- Packing in Cartons & Pallets
- 100% Polyester Ring Spun yarns of china origin available in natural raw white and dope dyed colors suitable for non-critical applications where quality is not important available in 2 fold, and also in multi fold- Ne10s to Ne 28s
Specifications :
100% Polyester Sewing thread raw white yarn :
| Quality Test Report |
- |
| Nominal Count |
NE 42/2 Poly 100% RT |
NE 20/2 Poly 100% RT |
| Fibre Psf/Vsf |
Sht fibre |
Sht Fibre |
| Quality Parameter |
- |
- |
| Act Count |
21.79 |
9.97 |
| Count C V % |
1.5 |
1.42 |
| Lea Strength |
285 |
663 |
| CSP |
6210 |
6610 |
| Yarn TPI |
22.51 |
16.05 |
| TPI CV% |
3.23 |
1.53 |
| Tenacity CN/Tex |
34.12 |
40.05 |
| Elqng % |
13.19 |
12.9 |
| Elong CV% |
6.33 |
4.8 |
| Yarn U% |
7.84 |
5.95 |
| Thin/KM |
0 |
0 |
| Thick /KM |
2 |
1 |
| Neps/ KM |
4 |
2 |
|
|
|
|
| |
|
|